Quote:
Originally Posted by Sean5294
Hi! Im new to the site and to polishing. I have been polishing motorcycle parts for a few months. I have a 6inch buffer and have been using eastwood compounds. here is a quick pick of some recent work.
They are levers from a 1983 Honda Nighthawk, i need to get something to get into the smaller spaces.
LAter!!!
|
Hi Sean. welcome. Good luck with the polishing - when you have questions, do a quick search in here so you get a few ideas, then feel free to ask.
If you're starting off cheap and simple (a good way), you might try some of these
http://www.caswellplating.com/buffs/sanding_drums.htm - you can use them in a drill and make your own drums if you want. There are many other methods for getting smaller areas, but these are a quick and smple way to get started.