Old 05-05-2003, 01:21 AM
ARP ARP is offline
Newbie
 
Join Date: Apr 2003
Posts: 1
ARP
Default polishing my GSXR frame

OK this website has me confused.In one area I'm told to use emory bar then tripoli bar.In another area I'm told to use a white rouge after tripoli.I've tried it all(black magic rouge,xtra dry cut/color compound,emory and tripoli)and can't get it right.I usually end up with a good shine but can't get rid of the streaks.Please let me know what the best method and product is so I can finish this project.Also,is clearcoat remover going to help surface prep?Thanks.
Reply With Quote
  #2 (permalink)  
Old 05-05-2003, 09:16 PM
Newbie
 
Join Date: Mar 2003
Location: Montreal, Canada
Posts: 19
gagnon
Default

First make sure that you remove any trace of clearcoat on your part to polish.

After that it depends how is the condition of your part, do you have deep scratch or it is free of deep scratch.

Always test buffing with softer compound before more agressif compound, you will save lots of time. For exemple try with Tripoli if it is not agressif enough go with emery. By the way Emery is more agressif then tripoli.

hope this will help.
good luck
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Frame polishing....same process...2 different finishes? HELP bairdmotorcycles Metal Polishing Questions 15 06-27-2005 03:13 PM
polishing frame shaybirde Metal Polishing Questions 4 04-23-2005 11:18 PM
lots of questions, polishing motorcycle frame nopulse95 Metal Polishing Questions 10 02-11-2004 12:39 AM
Polishing bike frame flyjetta Other Metal Finishing Questions 1 10-09-2003 01:19 PM
Frame Polishing Question SICKGIXX Metal Polishing Questions 10 03-18-2003 10:50 AM


All times are GMT -4. The time now is 07:50 AM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.