I am refinishing the exterior door handles off of a 1959 Ford. The handles a small cluster of pits that are not very deep but they can be felt and have small black centers. Other than the small concentrated pits, the remainder of the chrome seems to be in great shape. I was able to wet sand the raised pit area down on one of the handles, so it is now smooth, but the black centers remain. I will we only be using this car as a daily driver, so I do not require show quality plating. I would rather not strip off the good chrome, but instead re-plate the pitted areas. I have never worked with chrome before, so I am looking for something easy and low cost. Can this be done? How should I prep the areas? What kit or method should I use to re-plate? Moreover, how should I finish and buff out the entire handle? Thanks
  #2 (permalink)  
Old 05-14-2003, 10:02 AM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,357
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

Please don't cross post. This was answered in the plating forum.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Closed Thread

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
copy chrome vs triple chrome plating splbnd27 Electroplating Questions 18 06-21-2006 07:35 AM
Copy Chrome Start-up Elitefisherman Electroplating Questions 10 04-18-2004 04:24 AM
Chrome (re)plating question - howto olaf_sc Electroplating Questions 1 07-29-2003 02:00 PM
New to Chrome - Repairing Pits edseldude Plating Pot Metal 1 05-14-2003 09:55 AM
Repairing rusted chrome plating Angel Electroplating Questions 2 04-19-2002 10:13 AM


All times are GMT -4. The time now is 05:46 PM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.