Default Spotty Polished Wheels

I'm polishing a set of Zq8 wheels, and are almost finished. But, on the final polishing step. I seem to be getting some shadowing or ghosting affects. In the polishing manual from the website, it states to use corn starch or talcom powder. That isn't working. I've heard that it's caused from heat. How do I get rid of these spots? This is my third time polishing aluminum and have never experienced this before.
Suggestions.
Reply With Quote
  #2 (permalink)  
Old 05-21-2003, 10:36 AM
Amateur Metal Finisher
 
Join Date: Aug 2002
Location: Mississippi Gulf Coast
Posts: 133
marsfrogie
Send a message via AIM to marsfrogie
Default

Perhaps it is a heat problem? Normally if you buff those with white they will come out.
Reply With Quote
  #3 (permalink)  
Old 05-21-2003, 12:41 PM
Newbie
 
Join Date: Feb 2003
Posts: 2
dadszx7
Default

Thanks,
I'll try that. I'll send in some photo's of these wheels. They look awesome. I'll send in a photo of B-4 and after.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Need help polishing my polished aluminum wheels suparida Metal Polishing Questions 12 09-02-2005 10:08 AM
Cant get compound onto the wheels 1105 Metal Polishing Questions 3 04-28-2004 10:05 AM
Polishing truck wheels with minor corrosion karter03 Metal Polishing Questions 0 02-19-2004 04:04 PM
A ? regarding polishing aluminum wheels... geotexZ71 Metal Polishing Questions 4 04-25-2003 09:12 AM
Screwed up polished wheels, HELP PartTimer Metal Polishing Questions 4 07-10-2002 11:01 PM


All times are GMT -4. The time now is 03:11 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.