I'm buying a bench grinder and was going to order some suplies from this site, but I wanted to ask a few questions first.
Is it ok to use greasless compounds on the loose cotton wheels? I know it's best to use the harder wheels but I need somthing that can get into tight places. I know to use one compound per wheel, but it looks like most greasless kits( other supliers) come with 2 or 3 compounds and one wheel. Can you use one wheel for several greasless compounds? Thank you |
|
|||
|
I have heard that you can wash the wheels in soap and water. Not sure of how well it works though. Your compounds would only be as fine as the coarsest abrasive if you were not 100& sucessful in getting the old compound off.
|
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Buffing wheels and their compounds. Something not right. | L98-Z | Metal Polishing Questions | 7 | 01-21-2006 02:23 PM |
| Polishing stainless steel MC exhaust mid pipes | kevinw1961 | Metal Polishing Questions | 3 | 05-22-2005 09:28 PM |
| Need Help Polishing aluminum Wheels. | mattyp | Metal Polishing Questions | 13 | 06-14-2004 08:44 PM |
| Cant get compound onto the wheels | 1105 | Metal Polishing Questions | 3 | 04-28-2004 09:05 AM |
| Polishing sport bike frames. | mercsvt | Metal Polishing Questions | 2 | 03-10-2002 03:06 PM |