lloyd
Default copychrome

I have some new u-bolt nuts I want to copychrome. They have a black coating on them, I don't know what the coating is. I put them in sulphuric acid and they fizzed a little bit, but there is still a little black on them. I guess my question is, will there be a problem putting them in the copychrome, I don't want to ruin the solution? Of cource the outsides will be polished, but the threads will still have the black. Thanks for any help in advance. lloyd
Reply With Quote
  #2 (permalink)  
Old 08-03-2003, 04:21 PM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,357
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

It's probably a black oxide coating. It needs to come off before plating. Use muriatic acid. See http://www.caswellplating.com/bbs/viewtopic.php?t=643
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
  #3 (permalink)  
Old 08-03-2003, 08:46 PM
Newbie
 
Join Date: Jun 2003
Location: BUCKEYE,AZ
Posts: 16
lloyd
Default THANKS CASWELL

Thanks a bunch. I will give the muratic a try. lloyd
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
copychrome over silvaspray copierfixer Copy Chrome Kit Customers Only 5 04-11-2006 08:30 AM
Blasting onto a copychrome finish Dan2003 Other Metal Finishing Questions 1 11-17-2003 11:41 PM
Copychrome lloyd Electroplating Questions 2 10-07-2003 12:01 AM
Prep for copychrome lloyd Other Metal Finishing Questions 0 09-13-2003 09:24 PM
Copychrome lloyd Electroplating Questions 2 07-27-2003 07:02 PM


All times are GMT -4. The time now is 03:18 PM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.