Default Refinishing Metal Golf Club Heads

Preface - In the last few years golf club Drivers & Fairway Woods have changed from wood heads to metal heads. Fairway Woods are usually made out of stainless steel and most Drivers are made out of Titanium.

The clubs come from the factory with a beautiful painted finish and depending on the amount of play will soon become scratched and loose their desireability - not for play but just because they are so scratched up. Many are discarded prematurely for this reason

My Question - I am a golf club repair hobbiest and would like to find an efficient way to dye (or otherwise refinish) the metal. I can take off the paint and polish the heads in preparation to refinish and do a great job. My problem is the finish. Re-painting is a royal pain. I think you would have to really be set up to do several heads (at least 10) at once to make it worthwhile and I only would be doing 1-3 at a time - also, masking the heads and keeping them dust free is very difficult for an amateur's garage type setup.

By polishing the metal I can make them look great - even small nicks and scratches are removed. The problem is that very shiney metal isn't what a golfer wants because of the glare.

Any suggestions? Two thoughts (1) the dye would have to color uniformly and (2) it would be great (but not required) that the dye color could be sharply masked.

I think the most popular colors would be a graphite black and gun metal blue.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Golf Club Heads.. hvac36 Powder Coating Questions 3 02-21-2005 11:18 PM
golf club heads. skeleton Electroplating Questions 4 02-01-2004 12:22 AM
plating a golf club matt36887 Electroplating Questions 4 11-20-2003 03:45 PM
How would you go about restoring this stainles golf club? bryanfrew Metal Polishing Questions 0 11-07-2003 06:31 AM
Golf Heads garyw Powder Coating Questions 0 06-26-2003 12:03 PM


All times are GMT -4. The time now is 04:54 PM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.