I am a custom pen maker and am making a pen out of copper. I have applied Tiffany Green Oxidizer to the copper tubes. When I get the look I want how do I stop the oxidizers reaction? Is this going to be a durable finish and not wipe off with use or should I apply a lacquer coating to the tubes?
I am also going to be trying the Bronze & Blackening and the gun blue finishes for copper. Will they require a lacquer coating? Jim D |
|
||||
|
To stop the reaction, rinse in distilled water.
You can apply a clear lacquer over the part if you wish. Any clear lacquer, such as VHT, should work fine.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| arctic cat green, anyone have it | corybarta | Powder Coating Questions | 8 | 09-30-2008 09:23 PM |
| Green Chromate | steveparson | Electroplating Questions | 0 | 07-15-2005 12:19 PM |
| green dye | jamerson | Anodizing Questions | 4 | 06-26-2005 01:23 PM |
| Casewell LT sealer dye leech | blackcote | Anodizing Questions | 9 | 06-30-2004 12:11 PM |
| WHY IS OLICE GREEN ANODIZING ORANGE | Anzalon | Other Metal Finishing Questions | 1 | 01-11-2003 12:42 PM |