Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum  

Go Back   Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum > Other Metal Finishing Questions

Notices

Other Metal Finishing Questions Discussion board for any metal finishing questions not covered in the topics above.

Reply
 
Thread Tools Display Modes
  #1 (permalink)  
Old 10-20-2003, 02:14 PM
Experienced Metal Finisher
 
Join Date: Dec 2002
Location: NJ
Posts: 290
tomg552001
Send a message via AIM to tomg552001
Default Tank heater for SP degreaser

Where can i get tank heaters for my parts washing bins? SP degreaser needs to be heated and what would i use to do so? How hot and fast will the 15 inch 300w heat about 5 gallons worth of solution?
Reply With Quote
  #2 (permalink)  
Old 10-20-2003, 10:21 PM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,356
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

The ceramic heaters work very well for this application.

See http://www.caswellplating.com/suppli...c_heaters.html
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
  #3 (permalink)  
Old 03-23-2004, 01:43 AM
Newbie
 
Join Date: Mar 2004
Posts: 1
pigvomit
Default

I use a crock pot for small parts. If I need to do a part thats too big for the crock pot, I use aquarium heaters in a 5 gal tank.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
tank heater update from clydes clydes Electroplating Questions 2 02-16-2005 12:06 AM
Need opinions on my next tank. jtsuttle Anodizing Questions 4 03-29-2004 12:32 PM
plating tank setup confusion fxstcguy98 Electroplating Questions 5 01-28-2004 10:26 PM
pretreatment tank bzer1 Powder Coating Questions 6 01-22-2004 10:07 PM
Tank Heating Questions. meganine Anodizing Questions 1 08-03-2003 03:20 PM


All times are GMT -4. The time now is 03:58 PM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.