mikedinmd
Default attention: polygon

have read your tips for using sivachrome. do you have any other info you could share regarding the performance of this kit? is it difficult to get a good result? are the guns suppied with the kit a pita to use? i'm considering buying one of these kits and was wondering what your opinion is on using this kit to redo parts that wouldn't be feaseable to do with a plating kit. thanks for any help. mike diaz
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
HOBBY SHOP PLATERS ATTENTION... etcc Electroplating Questions 0 03-29-2005 08:38 AM
ATTENTION SUCCESSFUL PLATERS - YOUR DATA NEEDED mcaswell Electroplating Questions 4 03-02-2005 03:00 PM
Power supply follow up question: Attention Fibergeek Gabourie Electroplating Questions 7 09-25-2004 08:53 PM
Acid copper plating problem! Attention Fibergeek Gabourie Electroplating Questions 10 08-14-2004 11:24 PM
Attention "Pyro puttiers".... minord Other Metal Finishing Questions 0 06-13-2004 12:39 PM


All times are GMT -4. The time now is 12:32 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.