Default A385 Aluminum Blackener

I just purchaced some A385 Aluminum Blackener. When trying it out the part got nice and black, but rubbed right off after I rinsed it.

Does this product need some sort of sealer? Are instructions supposed to be included?
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Something for you die hard polishers out there to chew on thesound Metal Polishing Questions 15 12-03-2007 12:16 PM
Copy Cad kit - blackener and yellow cad durability problems Broke Electroplating Questions 11 01-09-2005 10:19 AM
Do you have to use flash copper to plate aluminum krsimulis Electroplating Questions 1 07-27-2004 01:32 PM
Aluminum polishing help needed erikchow Metal Polishing Questions 1 02-25-2004 02:44 AM
HELP! White haze when degreasing polished aluminum! davidh90046 Metal Polishing Questions 2 10-15-2002 01:19 PM


All times are GMT -4. The time now is 07:17 PM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.