That's what i was thinking. I should have my order of it Friday and the customer is suppose to get it back on sunday. That means i need to spray it has soon has i get it. Is it alright to use a rust preventive solution before it is sprayed?
|
|
|||
|
i didn't i blasted the part then coated ..... so i can't say yes or no to that one .... the rust pervent... has to be a high temp to or it will bubble off and take your coating with it .... i don't see any thing on the can about it either ..... if you do use it let me know what the out come is
|
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| High temp coatings | KeithLambert7 | Powder Coating Questions | 2 | 04-30-2005 04:25 PM |
| Cerakote Exotic Color Coatings | engineerscott | Powder Coating Questions | 4 | 11-28-2004 09:09 AM |
| Ceramic Coatings. aka Jet-Hot | Fireblade | Powder Coating Questions | 13 | 04-19-2004 08:57 PM |
| BN piston skirt coatings | FF | Electroplating Questions | 0 | 02-19-2004 10:56 PM |