Default penetrating sealer for black oxide

Is there any thing else that will work in place of the penetrating sealer for black oxide?
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Black Oxide protection 64dodge Other Metal Finishing Questions 2 08-16-2006 10:50 PM
Marine Grade Sealer reelpeeler Anodizing Questions 3 04-06-2005 09:11 PM
Black Oxide vs. Parkerizing ar15dcm Other Metal Finishing Questions 1 07-02-2004 01:59 PM
Casewell LT sealer dye leech blackcote Anodizing Questions 9 06-30-2004 12:11 PM
How Good is Black Oxide bhysjulien Other Metal Finishing Questions 9 05-24-2004 09:12 PM


All times are GMT -4. The time now is 02:27 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.