i\'ve got a bare aluminum bike frame that i\'ve
brushed with scotchbrite pads. i love the look, but if i touch the frame i get black residue. can i just spray it with clear coat or do i have to somehow \'clean\' the frame before painting? and i so, how?! Many thanks!! |
|
||||
|
Yes, you can clear coat it. See http://www.caswellplating.com/vhtclear.htm
You\'ll need to de-grease the part first with some lacquer thinner. Just follow the instructions on the can.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Something for you die hard polishers out there to chew on | thesound | Metal Polishing Questions | 15 | 12-03-2007 12:16 PM |
| Aluminum corroding under clear coat | pdeinc | Powder Coating Questions | 8 | 03-07-2005 01:04 PM |
| Can I powder coat polished aluminum? | remotestartdepot | Powder Coating Questions | 3 | 05-20-2004 11:00 PM |
| Aluminum prep for chrome plate | jm | Metal Polishing Questions | 1 | 02-02-2004 12:24 AM |
| Aluminum Wheel prep and polish | patrickzeus20 | Metal Polishing Questions | 2 | 03-04-2003 12:00 PM |