Default Removing copper plating? Help......

What is the best way to remove copper plating found under the nickel finish on some firearms? I am removing the copper to engrave and then renickel with Caswell's kit. Extremely happy so far! Thanks!
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
I did a dumb thing - now how do I remove copper plating? Mark3316 Other Metal Finishing Questions 0 05-19-2005 02:57 PM
Removing copper plating.......Help! Coltsaa Electroplating Questions 8 11-03-2004 11:34 PM
Differet copper plating questions, plus copy chrome/ nickel? krsimulis Electroplating Questions 1 07-26-2004 12:25 AM
Copper plating on stainless steel 316L strip/sheet slee36 Services Offered/Wanted 0 03-31-2004 12:46 PM
Silver Plating on Copper hparent Electroplating Questions 1 04-03-2002 05:16 PM


All times are GMT -4. The time now is 09:45 PM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.