How can you tell if plating is chrome or nickel? I'm working on an antenna mast off of a 66 corvette. I would like to refinish it with the original coating. I sanded an area thru to the brass and didn't visually see any intermediate plating.
|
|
|||
|
If you know how to dechrome, you will know the object is chrome plated if you get a yellowish color either in the dechroming tank or the anode if you are brush plating. Hope this helps.
|
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Nickel first before hard chrome? | Daveleeander | Electroplating Questions | 0 | 12-02-2004 11:13 AM |
| Differet copper plating questions, plus copy chrome/ nickel? | krsimulis | Electroplating Questions | 1 | 07-26-2004 12:25 AM |
| chrome or nickel? | txturbo | Electroplating Questions | 3 | 06-02-2003 12:23 PM |
| Chrome, Nickel or copy chrome? | dwthomas | Electroplating Questions | 1 | 02-15-2003 01:49 PM |
| Electroless Nickel over Chrome | gglines | Electroplating Questions | 1 | 05-12-2002 11:09 PM |