Well, I received my SilvaChrome kit and finally had a chance to do some testing with it today. I tired 2 different tests with it. The first one was a total disaster .... Then with some help for another member JDee, the second test went better. But still not the results that I need.
I was doing a that was about 4" X 6".

After applying the silver, it looked great in 75%, but there were some spots that had a brownish color.

Then after I gave it the final rinse with distilled water, it left some milky areas? I went ahead and tried to top coat it, and that is when it really went down hill. It immeadiatly turned goldish brown. I also got many spots that looked like the the silver was cracking under the clear.

The color was really bad after the clear.

Any other suggestions as to what to try? Also, thanks JDee for the help to day. I'm going to give it another try next weekend.

Dale
Reply With Quote
  #2 (permalink)  
Old 10-22-2002, 04:58 PM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,357
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

Post a problem report in PRS at http://www.caswellplating.com/support.htm and we'll help you out.

Thanks
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Some newbie questions... kiwijetpilot Anodizing Questions 16 03-12-2005 08:18 PM
Looking for others who have used Silvachrome non-stick Other Metal Finishing Questions 4 12-06-2003 10:19 PM
Air Compressor Recommendation - Silvachrome Therber Other Metal Finishing Questions 0 05-25-2003 06:56 PM
Silvachrome Question Hughesy Electroplating Questions 1 09-03-2002 02:14 PM
Silvachrome question Owen Electroplating Questions 10 06-20-2002 09:19 AM


All times are GMT -4. The time now is 11:33 PM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.