I bought some of the Phenol Novolac Sealer for a motorcycle tank and have a question before I apply it.
I made the tank from scratch out of sheetmetal that came with a protective coating (zinc?) Its a gray-ish color. I didn't remove the coating before making the tank, so now I'm wondering if it's OK to apply the epoxy sealer over this, or if I need to figure out a way to remove the coating. Thanks, Bret Portland, OR |
|
||||
|
This is probably a zinc plate.
I would suggest that you clean the zinc by running a 2% muriatic acid into the tank. This will etch the zinc and remove a great deal of it. Leave it in there for a minute, then rinse and dry thoroughly. Then apply the sealer
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
|
|||
|