| Notices |
| Other Metal Finishing Questions Discussion board for any metal finishing questions not covered in the topics above. |
![]() |
|
|
Thread Tools | Display Modes |
|
|||
|
I have an old mirror that I want to put on my truck but the problem is that its too nice. My old truck is original and either has worn, pitted or rusted chrome and this new mirror will stand out like a sore thumb! Is grinding or using an emery cloth still the best method for this?
Thanks, rick |
|
||||
|
If you sand it, the thing is probably going to rust like an old tin can. If that 's what you want, go for it.
Or, you could strip the chrome, using muriatic acid, to expose the nickel, which has a more antique look to it, and the stripping will dull the finish. The nickel will still afford corrosion protection.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
|
|||
|
Thanks. I know this post & question is kind of 'reverse' of what everyone is doing but in this specific case, it is. I love the products you sell and your powercoating paint is the best.
rick Last edited by 1958A120; 10-23-2005 at 10:23 AM. |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Need some help making RED fish hooks | nitro901 | Other Metal Finishing Questions | 2 | 03-27-2008 02:11 AM |
| making real money polishing? | saiyan7 | Metal Polishing Questions | 22 | 12-24-2007 04:41 PM |
| Making circuit traces on plastic parts. | Riesebosch | Electroplating Questions | 1 | 05-02-2005 02:49 AM |
| Making $ | FMXhellraiser | Powder Coating Questions | 17 | 07-04-2004 05:55 PM |
| Making electroless nickel look more like silver | rlforbes | Other Metal Finishing Questions | 1 | 02-16-2004 01:52 AM |