Default Can you dip Ceramic Coating.

Just wondering if it is possible to dip ceramic coating in a tank instead of spraying it?
Reply With Quote
  #2 (permalink)  
Old 02-22-2006, 09:42 AM
pickleboy's Avatar
Metal Finishing Guru
 
Join Date: Feb 2005
Location: belleville michigan
Posts: 635
pickleboy is just really nicepickleboy is just really nicepickleboy is just really nicepickleboy is just really nice
Default Re: Can you dip Ceramic Coating.

yes you can dip it but it is not the preferred way to do it. think about a flat sheet when you dip and pull it out the excess will start to run off. the coating at the top will be thinner than that on the bottom. if you want to do it so as to get the inside of header tubes, then the answer is yes but it will take a good amount to be able to submerse them. hope this helps bro.
__________________
when in doubt polish it out/ why replace it when you can refinish it
G2 Polishing and Powdercoating
Reply With Quote
  #3 (permalink)  
Old 02-22-2006, 06:26 PM
machone's Avatar
Amateur Metal Finisher
 
Join Date: Jun 2005
Location: White Lake Michigan
Posts: 93
machone will become famous soon enough
Default Re: Can you dip Ceramic Coating.

To get the inside, cap the end, pour coating in & turn the pipes to spread it, pour out excess, cure. try to use just enough, I think you will have adhesion problems if you reuse the excess. Tricky stuff!
mach
__________________
TSA Custom Metal Finishes
Live fast, Die sideways
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Ceramic coating dbug10 Oven Building Forum 4 03-06-2006 12:44 AM
Fs: Turnkey Powder Coating And Ceramic Coating Business!!!! Mcurtis7 Used Items For Sale 0 10-02-2005 02:18 PM
looking... yellow ceramic coating... MikeWalker Services Offered/Wanted 2 09-27-2005 09:34 AM
Ceramic coating for wear rclint Other Metal Finishing Questions 0 08-23-2005 10:23 AM
Ceramic Coating an Engine Block? thesound Powder Coating Questions 13 02-19-2005 07:37 PM


All times are GMT -4. The time now is 03:12 AM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.