Old 01-10-2003, 09:59 AM
Newbie
 
Join Date: Jan 2003
Posts: 1
Anzalon
Default WHY IS OLICE GREEN ANODIZING ORANGE

Anodized a bar of aluminum yesterday. Anodizing went perfectly. However, first time using the Olive green dye and it came out copper colored, burnt orange; not a spec of green in it! Is it possible the dye was mislabeled or is there some other issue? I can live with the color, but don't want it to happen again. Any suggestions?
Reply With Quote
  #2 (permalink)  
Old 01-11-2003, 12:42 PM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,357
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

Please post a problem report in our PRS system and we'll be able to help you troubleshoot what went wrong.

Thanks
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Orange Peel griffsfsr Powder Coating Questions 5 03-02-2004 11:24 AM
"Hard" Anodizing vs. "normal"; differenc dagobert Anodizing Questions 6 02-26-2004 11:24 PM
Color depth vs. anodizing time NeoMoses Anodizing Questions 17 02-03-2004 09:06 PM
Anodizing different alloys TONYZ Anodizing Questions 2 11-02-2003 01:31 PM
Titanium anodizing lorenzo Other Metal Finishing Questions 1 06-27-2003 08:56 AM


All times are GMT -4. The time now is 11:41 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.