Default Anodizing using RIT dyes Question

I was wondering if anyone had any different problems using different colors of RIT dye to color your anodized part?

I did a part the other night and used the Royal blue color on it and it turned out just fine, although it was a little more purple than I wanted.
But I did some parts last night, the exact same way I did the first ones but I used the dark green dye this time, and when I sealed the part almost all of it came off leaving a real light green when I wanted a dark green.

Are there differences in the colors that one will work better than the others?
I just ordered some dyes from Caswell today in hopes that will fix my problem.
Anyone know if the Caswell green is a real bright one?
Reply With Quote
  #2 (permalink)  
Old 01-20-2003, 12:27 PM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,357
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

It is a bright green, but color results are primarily a result of the anodizing process, rather than a problem with the dye.

Quality dyes (which ours are) will certainly help get results, but things like power and temperature during anodizing affect pore size, which affects dying.

If you have problems with the dyes you bought from us, open a Problem Report in our support section.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
  #3 (permalink)  
Old 01-22-2003, 12:22 AM
Newbie
 
Join Date: Jan 2003
Posts: 3
Hcues1
Default

I got the dyes today, man what a difference. I wont ever use RIT dyes again.
Reply With Quote
  #4 (permalink)  
Old 03-03-2003, 08:35 PM
Newbie
 
Join Date: Mar 2003
Posts: 3
pitotshock
Default

I have to say that the dyes I purchased from Caswell are first rate and are exactly what I wanted. I have been nothing but impressed with their results.

RIT dyes, well uhmm.... leave them at the grocery store
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Color depth vs. anodizing time NeoMoses Anodizing Questions 17 02-03-2004 09:06 PM
Anodizing different alloys TONYZ Anodizing Questions 2 11-02-2003 01:31 PM
opaque anodizing dyes july_favre Anodizing Questions 1 03-12-2003 08:26 PM
Anodizing using RIT dyes Question Hcues1 Anodizing Questions 1 01-20-2003 12:30 PM
dumb anodizing question felix Electroplating Questions 1 08-06-2002 08:37 AM


All times are GMT -4. The time now is 07:13 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.