Default Plated Aluminum

What is a good way to remove Chrome plating from Aluminum? I have a cold air intake pipe for my car that has numerous scratches and pitting, and I want to remove plating and polish out flaws. Will media blasting remove the plating and give me a good base to start the polishing process?
Reply With Quote
  #2 (permalink)  
Old 02-06-2003, 10:41 PM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,356
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

http://www.caswellplating.com/bbs/vi...=remove+chrome
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
  #3 (permalink)  
Old 02-08-2003, 12:54 PM
Newbie
 
Join Date: Feb 2003
Posts: 2
Bullitt 3309
Default

Will the acid harm the aluminum?
Reply With Quote
  #4 (permalink)  
Old 02-10-2003, 02:17 PM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,356
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

No it won't.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Something for you die hard polishers out there to chew on thesound Metal Polishing Questions 15 12-03-2007 12:16 PM
Need a couple of aluminum pieces plated: Dayton, Ohio area jmmyjam Services Offered/Wanted 5 06-16-2005 10:44 AM
Do you have to use flash copper to plate aluminum krsimulis Electroplating Questions 1 07-27-2004 01:32 PM
Can aluminum be satisfactorly BRUSH plated? GoldiesPlating Electroplating Questions 4 08-22-2003 09:09 AM
HELP! White haze when degreasing polished aluminum! davidh90046 Metal Polishing Questions 2 10-15-2002 01:19 PM


All times are GMT -4. The time now is 04:22 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.