Default Removing chrome to reveal nickel

I have a guitar bridge like this one:

It's chrome, but I would like it to be polished nickel to match the rest of the guitar's hardware.
I suspect the screws are steel, but other parts may be brass or pot metal.
How would you suggest I go about it?

Last edited by Chadd; 03-07-2007 at 02:57 PM.
Reply With Quote
  #2 (permalink)  
Old 03-08-2007, 04:50 PM
Newbie
 
Join Date: Mar 2007
Location: Los Angeles, CA
Posts: 4
Chadd is on a distinguished road
Default Re: Removing chrome to reveal nickel

And one other question: If I remove the chrome with muriatic acid, would the resulting nickel finish be shiny, or would it need polishing to make it bright? I'm not sure how I would polish all of those nooks and crannies.
Reply With Quote
  #3 (permalink)  
Old 03-20-2007, 08:38 PM
Newbie
 
Join Date: Mar 2007
Location: Los Angeles, CA
Posts: 4
Chadd is on a distinguished road
Default Re: Removing chrome to reveal nickel

Problem solved. Thanks for the help!
Reply With Quote
  #4 (permalink)  
Old 03-21-2007, 07:38 AM
Newbie
 
Join Date: Mar 2004
Posts: 15
tvsp
Default Re: Removing chrome to reveal nickel

For those of us gathering info, how was your problem solved?
Reply With Quote
  #5 (permalink)  
Old 03-21-2007, 12:13 PM
Newbie
 
Join Date: Mar 2007
Location: Los Angeles, CA
Posts: 4
Chadd is on a distinguished road
Default Re: Removing chrome to reveal nickel

The problem was solved by exchanging the chrome bridge for one with a nickel finish.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
removing chrome from pot metal without a blaster? customdrumfinishes Plating Pot Metal 4 08-20-2006 10:45 AM
Chrome and Nickel Removal Question (long) bentley86 Electroplating Questions 5 03-19-2006 04:32 PM
Removing the chrome surface from aluminum based auto trim jbashaw Metal Polishing Questions 6 10-01-2003 10:20 PM
Chrome, Nickel or copy chrome? dwthomas Electroplating Questions 1 02-15-2003 01:49 PM
Removing small scratches from Chrome mlust Metal Polishing Questions 3 10-06-2002 03:34 PM


All times are GMT -4. The time now is 04:37 PM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.