Default Black Oxide sealer not drying

We have the Black Oxide kit. I have not used it much but I now have decided to use it on all the tools I make and sell. The black looks fine but after it is dipped in the sealer it will not dry but stays slimy. It has been hanging to dry for over 12 hours and it is still wet. If you touch it it smears.
What am I doing wrong?
Reply With Quote
  #2 (permalink)  
Old 08-25-2007, 07:38 PM
destroyer125's Avatar
Experienced Metal Finisher
 
Join Date: Jul 2005
Posts: 425
destroyer125 is an unknown quantity at this point
Default Re: Black Oxide sealer not drying

I never could get the stuff to work. The black finish always rubbed off. Its nothing compared to the real black oxide process.
Reply With Quote
  #3 (permalink)  
Old 09-27-2007, 09:29 AM
Newbie
 
Join Date: Jun 2004
Posts: 1
brucearnn
Default Re: Black Oxide sealer not drying

Huh, I use it all the time and prefer it as a good finish for low cost. I was hoping you guys would tell me how to improve on my process. Here's how I do it:
1) get the part clean - wire wheel and rubbing alchahol.
2) get the acid hot - a crock pot works best.
3) keep the acid strong and clear of white dust - I use a funnel and coffee filters but there's probably a better way.
4) a fish tank bubbler helps move things around.
5) dip time should be about 3 to 10 minutes (depending on strength of acid) remove from acid and dip in tap water.
6) dab or rolle the part up in a towel - do not wipe it dry.
7) immediately (within 30 seconds) get the part dipped in oil - lay them out to dry. They won't dry - if the part does dry, you've made a mistake.
wait at least 24 hours, 3 days is better. Wipe off oil residue - done.

Other trivia - cut up some 6 in pieces of romex copper electrical cable. Each of piece isulated copper wire makes an easy adaptable hanger. Strip the insulation or throw in a piece of copper if you want a bronze tinge to the color.
Bruce
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Need Help w/ Black Oxide Kit salezdroid Other Metal Finishing Questions 3 11-18-2004 06:54 AM
penetrating sealer for black oxide jtsuttle Other Metal Finishing Questions 0 05-21-2004 09:00 AM
black oxide bonesmachine Other Metal Finishing Questions 1 06-02-2003 12:03 PM
black oxide sswhite Electroplating Questions 1 04-06-2003 02:52 PM
Black Oxide L98-Z Other Metal Finishing Questions 1 08-01-2002 11:33 PM


All times are GMT -4. The time now is 06:52 PM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.