I just ceramic coated my exhaust turbo housing. I baked it on per the instructions. Once it ws dont i hit it with #0000 steel wool. It looks great. I also read to apply a polish to keep the shine. What polish? Wont the polish change color once this heats up on the car?
Thanks, Chris |
|
||||
|
If you want to treat with a polish I would suggest the Glare Professional Polish. It is applied in two coatings; first you rub in until it disappears then apply a second coat allow to dry to a haze then buff. Please check this link: http://www.caswellplating.com/aids/glare.html
__________________
-- Craige Brooks Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| where to buy ceramic coating | InfernoCoatings | Powder Coating Questions | 7 | 02-25-2008 10:50 PM |
| Polishing ceramic coating | callmej75 | Metal Polishing Questions | 0 | 04-23-2006 10:12 PM |
| Ceramic coating | dbug10 | Oven Building Forum | 4 | 03-06-2006 12:44 AM |
| Can you dip Ceramic Coating. | gestalt | Other Metal Finishing Questions | 2 | 02-22-2006 06:26 PM |
| Fs: Turnkey Powder Coating And Ceramic Coating Business!!!! | Mcurtis7 | Used Items For Sale | 0 | 10-02-2005 02:18 PM |