I have some clear anodized motorcycle parts that I want to paint, do I need to remove the anodizing first, if so what product do you recommend, if not how should I prepare the surface for paint and do I need a special primer?
|
|
||||
|
You don't need to do anything special to paint it. Just paint it.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Something for you die hard polishers out there to chew on | thesound | Metal Polishing Questions | 15 | 12-03-2007 12:16 PM |
| cleaning anodized aluminum | rancidnsx | Anodizing Questions | 0 | 01-26-2005 11:56 PM |
| Procedure to strip anodized layer off aluminum. | remarc1 | Other Metal Finishing Questions | 1 | 07-27-2004 04:41 PM |
| anodized aluminum pore dimension | sam4 | Anodizing Questions | 2 | 03-11-2004 07:57 AM |
| Chroming anodized aluminum. | hifi | Electroplating Questions | 4 | 08-05-2003 12:23 PM |