I want to get a wear resistant Electroless Nickel plating on Aluminum. What will be the difference between med phos and high phos pretreatment in my case, please? Which one is better? Is the difference significant or not? What kind of literature can you recommend?
Thank you.

Andrei
Reply With Quote
  #2 (permalink)  
Old 04-30-2003, 03:04 PM
mcaswell's Avatar
Caswell Inc Founder
 
Join Date: Nov 2001
Location: Lyons, NY USA
Posts: 2,359
Blog Entries: 1
mcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to beholdmcaswell is a splendid one to behold
Default

Try posting this question on finishing.com. We don't deal with these sorts of applications, so don't know too much about them.

Another good source of EN info is http://www.sirius-tech.com
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


All times are GMT -4. The time now is 03:34 AM.


Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0
Copyright © Caswell Inc.