I am interested in darkening my brass faucet. It is solid brass and I imagine it has a protective coating.
Can you recommend a removal process for the protective coating? It indicates that the products be used as a dip, but I am VERY wary of removing this faucet to darken it. Any way to use as brush on/wipe off? Or would this be uneffective? Thanks! Jodie |
|
||||
|
Clearcoat remover should remove any protective coating. See http://www.caswellplating.com/aids/clearcoat.htm
The issue is keeping the entire part coated with the solution until you get the desired finish. If there are parts of the faucet that the solution runs off of, you'll end up with a very patchy looking finish.
__________________
-- Mike Caswell Caswell Inc http://www.caswellplating.com Need Support? Visit our online support section at http://support.caswellplating.com Have A Web Site? Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Restoring coated brass rails? | trsick | Metal Polishing Questions | 6 | 04-14-2005 11:29 PM |
| Brass Plating Tank | agugliel75 | Electroplating Questions | 7 | 02-06-2004 09:50 AM |
| Clearcoating brass after polishing | skipmac | Metal Polishing Questions | 1 | 10-04-2003 09:58 AM |
| Brass Weathered Finish Look/Antique Brass | agugliel75 | Metal Polishing Questions | 2 | 06-21-2003 09:09 AM |
| Uh-oh, where'd the brass go? | jtowens | Metal Polishing Questions | 1 | 02-07-2003 03:17 PM |