First post!

I have some small gun parts, ie butt plates that are made of AL. They were painted but scratched easily, showing the silver. Is there a inexpensive DIY way to oxidize these with a black color?
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
Reply With Quote
  #2 (permalink)  
Old 12-21-2008, 10:35 AM
lcaswell's Avatar
Caswell Inc President
 
Join Date: Jan 2001
Location: Lyons NY USA
Posts: 2,461
Blog Entries: 3
lcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud oflcaswell has much to be proud of
Default Re: Making AL black?

Aluminum Blackener - Caswell Inc. - Metal Finishing Solutions
__________________
--
Lance Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm

Please support the moderators on our site by leaving reputation for their helpful posts. Read more here.
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
Reply With Quote
  #3 (permalink)  
Old 02-05-2009, 10:20 AM
Newbie
 
Join Date: Jan 2009
Location: Janesville, WI
Posts: 28
ddrink is on a distinguished road
Default Re: Making AL black?

Does anyone have any pics for Al finished with blackener? I'm interested to see the finished look.

Thanks

Dan
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


Similar Threads
Thread Thread Starter Forum Replies Last Post
WHITE COMPOUND IS MAKING PART DULLER THAN THE BLACK HELP.... 03BUSABOY Metal Polishing Questions 5 02-02-2009 08:38 PM
Could use a little help making decisions osobob Powder Coating Questions 1 11-26-2007 04:33 AM
Homemade chiller in the making destroyer125 Anodizing Questions 30 08-02-2006 12:43 PM
Making an oven and ive got a few questions Tofurkey Oven Building Forum 10 07-18-2006 11:30 PM
Making $ FMXhellraiser Powder Coating Questions 17 07-04-2004 06:55 PM


All times are GMT -4. The time now is 04:17 PM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2009, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.3.0
Copyright © Caswell Inc.