Default BO Kit Question

I am planning on using black oxide on the barrel of a rifle I am refurbing and have a couple questions. Currently all parts that are to be oxided have been glass beaded. All parts are mild steel.


Does the sealer in the kit prevent rusting or will I have to apply oil to the piece from time to time?

Does caswell have a suggested tank/tray that will accomodate a 30 to 36 inch barrel?

Anything else I need to know?

Thanks
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
Reply With Quote
  #2 (permalink)  
Old 01-05-2009, 08:35 PM
Newbie
Caswell Platinum Member
 
Join Date: Jan 2005
Posts: 1
AMCDude
Default Re: BO Kit Question

I don't know what Caswell suggests, but I use a plastic storage container, the kind that is used for storing wrapping paper. It's about 36" long, works fine. You might have to swirl the liquid for complete coverage, but it can be done. You could use some vinyl gutter, with end pieces glued on, if you need something longer. Take a walk thru some discount stores, you'll be suprised w/ what you can get, cheap.

Last edited by AMCDude; 01-05-2009 at 09:12 PM.
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
Reply With Quote
  #3 (permalink)  
Old 01-06-2009, 03:28 PM
VinS's Avatar
Newbie
 
Join Date: Jan 2009
Location: Connecticut
Posts: 2
VinS is on a distinguished road
Default Re: BO Kit Question

Great, thanks.
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off



All times are GMT -4. The time now is 11:50 PM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2009, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.3.0
Copyright © Caswell Inc.