    So I have been building my spray booth for powder coating. and thought that I would share how i'm doing it. There's not many people that show what they did so I thought why not. after the booth is finished I will start building my LPG or CNG powered oven that will coat sand rails and other things of mass size. As for the oven that I have now its 5'W x 4' H x 3' L and its LPG powered and I got it for $50 so I can't bitch about that.

    As for the booth i'm building it's 5'W x 8' H x 4' L.

    I have 2 blowers attached to it. One came from a house furnace, It flows about 2000 CFM, As for the other blower that I have they clame that it flows 1725 CFM I dont know if I believe that but its clamed to. I think that I have spent a total of $60 dollars building this booth. Any input is welcome.

    Now let me see if I cant get the pictures to upload, sorry if the pictures are huge



    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  2. #2

    Default Re: building my spray booth with pictures.



    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  3. #3

    Default Re: building my spray booth with pictures.



    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  4. #4

    Default Re: building my spray booth with pictures.



    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  5. #5

    Default Re: building my spray booth with pictures.



    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  6. #6

    Default Re: building my spray booth with pictures.



    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  7. #7

    Default Re: building my spray booth with pictures.



    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  8. #8

    Default Re: building my spray booth with pictures.



    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  9. #9

    Default Re: building my spray booth with pictures.



    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  10. #10
    Join Date
    Feb 2006
    Location
    Bristol, In
    Posts
    718

    Default Re: building my spray booth with pictures.

    Been there and done that, a couple of times. Mine works well, better then dust all over. Appears that a lot of thought went into yours, meaning you were busy. Captions with the pics would help for those who want to put one together. I'm curious about the two fans and the purpose of two.
    Who says you can't teach an ole dog new tricks?
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

+ Reply to Thread
Page 1 of 2
1 2 LastLast

Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

     

Similar Threads

  1. Building spray / polishing booth
    By Ozz in forum Powder Coating Questions
    Replies: 6
    Last Post: 08-28-2009, 09:55 AM
  2. Building a spray booth
    By MarkC in forum Powder Coating Questions
    Replies: 2
    Last Post: 04-17-2009, 12:16 PM
  3. building a spray booth
    By daveg in forum Powder Coating Questions
    Replies: 13
    Last Post: 06-06-2008, 03:20 AM
  4. Building spray booth - a few questions:
    By bradnailer in forum Powder Coating Questions
    Replies: 4
    Last Post: 11-19-2007, 09:42 AM
  5. Building Sandblast Box and spray Booth
    By FiReBReTHa in forum Powder Coating Questions
    Replies: 26
    Last Post: 06-06-2007, 07:37 PM

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts

Search Engine Friendly URLs by vBSEO 3.5.0 RC1 PL1