call around to local construction suppliers. they should have it or be able to get it.
Where would you find this in Canada ?
Thanks
ian.
call around to local construction suppliers. they should have it or be able to get it.
Hi. I live in the beautiful Annapolis Valley. Nova Scotia.
I foind a place for the netal. 20 guage gal $ 100.00 4*8 sheet...I thought it was @ 32.00 most places.
Ian.
here is a link to roxul canada s distributors for rockwoolhttp://www.roxul.com/residential/where+to+buy+roxul
Thank-you very much.
Ian
Steel has gone up in price terribly in the past two years. although $100 for a 4X8' sheet sounds high. I went to a sheet metal shop with my exact dimensions and had all the 20 ga. sheet metal cut at the same time. It was for a 2' X 3' X 6' oven and the whole thing cost $295 plus tax. That was four years ago, however. It would be considerably more now.
Doing it as I did, I had no chance of cutting myself and nothing left over. You might want to contact a sheel metal shop and see what they would want for the job.