Results 1 to 2 of 2

Thread: Refridgerator PC Oven build info

  1. #1
    pcbeachrat is offline Newbie
    Join Date
    Nov 2009
    Posts
    6

    Talking Refridgerator PC Oven build info

    I was cruising through the threads here for I am now trying to build A PC Oven and seen a couple make them from refridgerators..With all the plastic in them now days I realize this will have to be gutted out..but does anyone have any plans for a fridge oven build? Or any specific info would be appreciated in this build. I have A sandblasting cabinet I built from a full sized fridge, but we have no heat involved in that build. I was looking around for tin, stainless and all other options in the local salvage yards the last few days, but have not found anything satisfactory as of yet...Fridges I run across no less than 3 or 4 weekly out at the curb sides. I want A bigger unit but A fridge unit would do for awhile just to play around wth..I have never even touched A PC gun as of yet, but fixing to learn..any pertinant info on a fridge oven build would be greatly appreciated...I have been coming to Caswells for A few months now concerning sandblasting mostly, and finally have decided to get into powder coating as well..Thanks..Great Group here..and tons of info!!

  2. #2
    ed_denu is offline Metal Finishing Guru
    Join Date
    Jul 2006
    Posts
    1,144

    Default Re: Refridgerator PC Oven build info

    If you just want to get started in pc, you might look for a kitchen oven. These are often found for free, same as the fridges you have found.

    IMO building an oven from anything such as file cabinets, refrigerators, etc. is more trouble than it's worth. They all need to be framed either on the inside or out and insulated, so why not just get some metal studs and build to the dimensions you desire.

Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

Similar Threads

  1. Good oven shell for wanting to build your own oven
    By dannydone in forum Powder Coating Questions
    Replies: 7
    Last Post: 09-13-2010, 12:32 PM
  2. New Oven Build
    By frankle8 in forum Oven Building Forum
    Replies: 6
    Last Post: 06-28-2009, 01:48 PM
  3. oven build q's
    By j4str in forum Oven Building Forum
    Replies: 4
    Last Post: 04-12-2009, 02:41 PM
  4. Anyone With A Used Oven Or Can Build A Oven For Me, Ohio
    By REVS in forum Oven Building Forum
    Replies: 2
    Last Post: 01-04-2008, 11:15 AM
  5. How to build an oven
    By Sezer in forum Oven Building Forum
    Replies: 2
    Last Post: 12-24-2003, 03:42 PM

Tags for this Thread

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •