| Notices |
| Oven Building Forum Building A Curing Oven? - Here's the place to post your questions, specs and ideas. |
![]() |
|
|
Thread Tools | Display Modes |
|
||||
|
I got the Idea from this dude. But I'm a fat dude so I wanted to make it upright. I used a old cabinet like you would see in a old school and the barn door track things real cool. That was my idea. I'm new to this site I hope you can see the pics.
http://www.powdercoatoven.4t.com/Index.html |
|
||||
|
If you have any questions e-mail me at mikekozura@yahoo.com
|
|
|||
|
Mike,
Don't know where you're out of but you should have an electric motor shop somewhere close by. The usually carry some small motors and small fan blades. We used a cheap air over 1/16 hp motor a 5 or 6" fan blade inside the cabinet. Shaft goes through the side wall and mounted the motor outside the cabinet. We got one with the shaft plenty long and mounted a 4" fan blade and 2" (cut down a 4") fan on the shaft between the cabinet and the motor. The inside one circulates the air and the 4" blows air over the motor and the 2" acts like a heat sling. Motor has been chugging away for 2 years, the works cost about $50.. The motor shop can help you pick the motor and blade so you get the rotation and correct blades.. Hope that helps |
|
||||
|
I'm live 20 miles south of Pittsburgh, PA. baby home of the World Champs. HERE WE GO STEELERS HERE WE GO. Thanks for the info I got some things brewing in my head now and that was a big help. Don't know where your from but I hope your a STEELER fan. LOL
This site has been a lot of help at least people will talk to you. I bought some powder from Pendry and was on there site and no one would talk to me. This powder coating and polishing is just like anything else common sense, practice, and what works for you. But its nice to have somewhere to turn for a opinion from someone that knows what the h@ll there doing. Thanks again. |
|
|||
|
I've got to agree with you, pretty sociable bunch here and some very knowledgeable members too.
We're situated about 50 miles due South of Cleveland. Not much of a football fan anymore but I can tell you when the Browns and Steelers play I know who will win |
|
||||
|
Quote:
Hey, I got a good idea who would win too. HERE WE GO STEELERS HERE WE GO Well I have to go and put some powder on some quad parts. Talk to you later. Last edited by mikekozura; 02-11-2006 at 01:19 PM. |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Cooking up an oven project... | dagobert | Powder Coating Questions | 33 | 06-09-2008 03:43 PM |
| advice on oven propane or electric | RCC | Powder Coating Questions | 13 | 11-26-2006 09:57 PM |
| Oven problem !!!!! | tavo1765 | Powder Coating Questions | 7 | 10-06-2005 05:21 PM |
| Newbie and oven temperature ? | Netnut | Powder Coating Questions | 2 | 05-26-2005 09:49 PM |