i have a standard household oven .ive removed the door and extended it another 3ft. with 22gauge metal.,boxed the front re-hung the original door ,isulated it. will the statdard element be enough to get to pc temp.i have the top broil element ,should i wire it to stay on with the bottom baking element?
|
|
||||
|
The single element will not be enough. Here is what I did with mine and it works great. http://forum.caswellplating.com/show...0846#post20846
Jason |
|
|||
|
Quote:
|
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| Cooking up an oven project... | dagobert | Powder Coating Questions | 33 | 06-09-2008 04:43 PM |
| Oven Heating Problem | petshe25 | Oven Building Forum | 18 | 02-26-2006 01:06 PM |
| Oven problem !!!!! | tavo1765 | Powder Coating Questions | 7 | 10-06-2005 06:21 PM |
| Custom oven material and heating element help needed | DarinReiss | Oven Building Forum | 13 | 12-27-2003 10:24 PM |