Default help wiring issure

can i splice the broil element wiring into the bake element wiring?
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #2 (permalink)  
Old 04-11-2006, 09:06 PM
Newbie
 
Join Date: Nov 2005
Posts: 6
dpmphoto is on a distinguished road
Default Re: help wiring issure

yes u can if you wish
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #3 (permalink)  
Old 04-11-2006, 09:32 PM
pickleboy's Avatar
Metal Finishing Guru
 
Join Date: Feb 2005
Location: belleville michigan
Posts: 636
pickleboy is just really nicepickleboy is just really nicepickleboy is just really nicepickleboy is just really nice
Default Re: help wiring issure

the only concern i can think of in doing so is will the contactor on the original controls have the amp capacity to handle both at the same time. if this is a self cleaning oven then it is ok. most modern ovens that are self cleaners use both to do so. otherwise they use one or the other.
__________________
when in doubt polish it out/ why replace it when you can refinish it
G2 Polishing and Powdercoating
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
  #4 (permalink)  
Old 03-15-2008, 07:08 PM
Newbie
 
Join Date: Oct 2006
Posts: 8
jnk-byr is on a distinguished road
Default Re: help wiring issure

The original controls can handle 3 elements but 4 is too many
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
Closed Thread

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


Similar Threads
Thread Thread Starter Forum Replies Last Post
Wiring a simple two element oven... wamontgomery Oven Building Forum 1 03-19-2006 03:49 PM
Help w/oven wiring! Deecoat Powder Coating Questions 3 09-14-2005 07:59 PM
Oven Wiring Noob2PC Powder Coating Questions 2 02-23-2005 02:34 PM
Wiring 101 :) hvac36 Powder Coating Questions 3 12-23-2004 04:58 PM
Powder coating oven suggestion (wiring) tomg552001 Oven Building Forum 1 04-22-2004 02:02 PM


All times are GMT -4. The time now is 06:42 PM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2009, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.3.0
Copyright © Caswell Inc.