With help from the one posted on the 28th, I was able to update mine and add a couple of items. I installed a 2 amp fues between L1 and L2 to protect the circuirty in my temperature controller.
I have 3 switches on my element circuit so that I can select which elements I want to use.
The motor wiring is still rough as I am waiting for the delivery of my 3 position switch and then I'll update it and include the wire color circuits and the starting capacitor circuit.
Can't figure out how to post a .bmp, If you'd like to see it email me and I send you a copy.
Glen