Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum  

Go Back   Plating Powder Coating Buffing Anodizing - Caswell Inc. Metal Finishing Forum > Powder Coating Questions > Oven Building Forum

Notices

Oven Building Forum Building A Curing Oven? - Here's the place to post your questions, specs and ideas.

Reply
 
Thread Tools Display Modes
  #1 (permalink)  
Old 02-01-2007, 09:46 PM
JTW37's Avatar
Metal Finishing Guru
Caswell Platinum Member
 
Join Date: Feb 2006
Location: Bristol, In
Posts: 514
JTW37 is an unknown quantity at this point
Default Sick and tired

Man am I ever sick and tired of that kitchen oven. Every time I attempt to put something in it after spraying, I either touch it or it bumps somewhere inside of the oven. Sure glad I started building my BIG oven. Can't wait till I get that done.

Mine is going to be 3'x3'x6' standing, when it's done. Am planning on three 2700 watt elements, the contactor that most of you are using, with a Berger-Coleman controller. Are the elements going to be enough or should I add another one?

Also want to have lighting in the oven and a door glass. I have noticed that many do not have this. Is it necessary to have the glass or no? Some of the powder says after it flows all over then lower the temp. How else would you know, without opening the door?
Thanks, JT
Reply With Quote
  #2 (permalink)  
Old 02-02-2007, 09:46 AM
nuttyman's Avatar
Metal Finishing Guru
 
Join Date: Sep 2003
Location: Rio Rancho, NM
Posts: 553
nuttyman
Default Re: Sick and tired

those elements will be enough for 54 cubic ft. the lightnig & glass is of course optional & is not necessary, but since you are building an oven you might as well do it right.
Reply With Quote
  #3 (permalink)  
Old 02-05-2007, 07:22 AM
JTW37's Avatar
Metal Finishing Guru
Caswell Platinum Member
 
Join Date: Feb 2006
Location: Bristol, In
Posts: 514
JTW37 is an unknown quantity at this point
Default Re: Sick and tired - But getting better

The reason I was thinking about the lights and the glass to view the parts, is because the powder instructions says "after flow out". How would you know if it has flow out without a glass? Other then opening the door to look, then you've lost a lot of the heat.

What other way would you know if you have flow out. You can't just trust time, right? Besides, if you see that it isn't going as planned, you could pull it before it totally cures, I would think.

I still fairly new at this game, so I don't know all of the in's and out's of powder coating and may never know them all, I'm sure. That's what is so great about this forum, many people here have been there and done that.

Thanks, JT
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


All times are GMT -4. The time now is 03:29 PM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.