Default Fan question for a fridge oven

What motor are you guys useing for the fan ,, Link would be most helpful
Reply With Quote
  #2 (permalink)  
Old 05-08-2007, 09:53 PM
JTW37's Avatar
Metal Finishing Guru
Caswell Platinum Member
 
Join Date: Feb 2006
Location: Bristol, In
Posts: 517
JTW37 is an unknown quantity at this point
Default Re: Fan question for a fridge oven

I bought mine used. A convection oven fan. Sorry no links.
__________________
Who says you can't teach an ole dog new tricks?
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Cooking up an oven project... dagobert Powder Coating Questions 33 06-09-2008 03:43 PM
Wood Charcoal oven? chromo Oven Building Forum 6 05-17-2007 01:11 PM
Oven Glass Question JTW37 Oven Building Forum 12 02-18-2007 01:01 AM
Question for all gas oven owners getastro Powder Coating Questions 3 06-16-2005 11:35 AM
building a oven question Jay87T Oven Building Forum 3 03-01-2004 05:28 PM


All times are GMT -4. The time now is 10:42 PM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.