Default Re: Wire size?

The material for the wire is definately different, but they take this into account when assigning the "guage".

For example: 14ga aluminum wire is larger than 14ga copper wire as aluminum isn't as good of a conducter.
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
Closed Thread

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


Similar Threads
Thread Thread Starter Forum Replies Last Post
wire spicing Deecoat Oven Building Forum 0 07-27-2006 10:12 PM
Braided wire kingkat Electroplating Questions 1 04-09-2006 05:31 AM
How do I wire up a 220 to my box? Hodges Oven Building Forum 3 10-25-2005 11:38 PM
where to buy aluminum wire jtsuttle Anodizing Questions 1 03-21-2005 04:42 PM
wire rims craigcraig Powder Coating Questions 3 07-03-2004 08:05 PM


All times are GMT -4. The time now is 06:48 PM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2009, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.3.0
Copyright © Caswell Inc.