  #21 (permalink)  
Old 10-25-2007, 08:37 AM
Amateur Metal Finisher
 
Join Date: Feb 2007
Location: Oklahoma City
Posts: 53
GeneNewcomb is on a distinguished road
Default Re: oven help anybody??

You can't build that oven for $400! Not even if your labor has no value at all.
Reply With Quote
  #22 (permalink)  
Old 10-25-2007, 09:34 AM
Amateur Metal Finisher
 
Join Date: Jan 2005
Posts: 96
holeshot87
Smile Re: oven help anybody??

i build a 6'hx4'wx4'd for around 400.00. thats everything.it heats up to 400 degrees in around 10 to 12 min.
Reply With Quote
  #23 (permalink)  
Old 12-08-2007, 12:41 PM
Newbie
 
Join Date: Nov 2007
Posts: 40
jw450r1 is on a distinguished road
Default Re: oven help anybody??

wow prices must have come down on metal.i priced out just the sheet metal for a 4x4x6 oven during the summer and it was close to $700..,elements were about $25.00 each.1000 degree insulation was abot $150.wiring was cheap.thats not including controls,handles,fan,light,sqaur tubing for the frame.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
My oven SCHEMATIC...for new oven builders.. RNMHRD Oven Building Forum 39 05-09-2007 05:18 PM
Good oven shell for wanting to build your own oven dannydone Powder Coating Questions 6 03-21-2006 10:40 PM


All times are GMT -4. The time now is 06:50 PM.


Powered by vBulletin® Version 3.7.2
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.