Default oven parts Q:

hi all newbie here, im working on a 4' x4' x6' oven much like 'krusty2111us's' oven (by the way anyone know how to get ahold of him i have some Q for him about his build)... Q: i have is about all the electrical components? i know this has been ask a million time but, i'v been reading and searching evrything i can but an still at a bit of a loss... im going to use a 'pid' controller, and 3 elements but from there?? i draw a blank. im good with the nuts and bolts of the thing just not the electrical end of things that when i need it spelled out in black and white!!! any body tell me where to start and/or what i should use!!!! thanks panman
Reply With Quote
  #2 (permalink)  
Old 11-04-2007, 09:08 AM
Amateur Metal Finisher
 
Join Date: Jul 2006
Posts: 222
ed_denu is on a distinguished road
Default Re: oven parts Q:

Panman, It would help if you could ask more specific questions. If you are totally new to electronics and wiring you might need to find someone to help you with this aspect. As these ovens typically use 120 and 240 VAC there is a real danger involved if they are not wired correctly.

Lookup some of the wiring diagrams posted here and see if that doesn't help get you started.
Reply With Quote
  #3 (permalink)  
Old 11-07-2007, 09:22 AM
grommit's Avatar
Amateur Metal Finisher
 
Join Date: Mar 2006
Posts: 208
grommit will become famous soon enough
Smile Re: oven parts Q:

Hello PANMAN, it is a very daunting task if you are like me and a totally no good with electrics. i can symathise with you as i searched and searched and by the end i was still not sure what all the 'Electric Speak' meant to me, don't get me wrong i understood what a PID,SSR etc now do but there is too much technical jargen it puts you off.
there are a lot of experts out there who can help and simplify the jargon for you, even PM'ing them if you are not happy asking on the forum (which i would encourage you to do)
i have my donor parts to fit this weekend, which i am lucky i have an electrician at hand for that, i am really happy i have took the plunge to start and make my own instead of hope one came for sale or even ask if someone can make me one.
i am in the UK but i have wiring Diagrams from the US that king people have emailed me.
check your PM's as i have asked for your email so i can send them to you if the persons who sent me don't object.
take care and good luck.
Brian
Reply With Quote
  #4 (permalink)  
Old 11-07-2007, 02:40 PM
Newbie
 
Join Date: Nov 2007
Posts: 5
54PANMAN is on a distinguished road
Default Re: oven parts Q:

Hey Grommit i pm'ed ya thanks for the help
Reply With Quote
  #5 (permalink)  
Old 11-09-2007, 08:10 AM
grommit's Avatar
Amateur Metal Finisher
 
Join Date: Mar 2006
Posts: 208
grommit will become famous soon enough
Smile Re: oven parts Q:

hello friend,
sent them by email last night (UK time) as i said in the email i hope they help, but i am no expert, it was the kindness of the other guys who passed them onto me.
catch you soon.
Brian
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
oven parts help needed grommit Oven Building Forum 10 10-15-2007 03:57 PM
Powder Coating oven parts. mtumbleson Oven Building Forum 7 03-06-2007 08:56 AM
Oven Parts and Numbers edwardpic Oven Building Forum 1 02-16-2006 11:48 AM
which parts to scavange from a household oven?? gestalt Oven Building Forum 1 12-01-2005 10:06 PM
Anyone have a good place online to purchase oven parts? tomg552001 Oven Building Forum 1 01-02-2004 08:34 AM


All times are GMT -4. The time now is 04:12 PM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.