Old 11-21-2007, 07:31 PM
Newbie
 
Join Date: Aug 2006
Posts: 20
olddude is on a distinguished road
Default Hey guys.....

I haven't been around for awhile and was wondering if anybody might know where would be a good place to maybe sell my big oven I built. I lost the lease on the building I was at and now I have no place to put it.

The oven is pretty much complete but there are a few finishing touches that need to be done. I have a ton of money tied up in this thing and I hate to have to srink wrap it again and sit it outside at my house.

It's a monster so it's not that easy to move around. Right now I have it stored at a friends shop but I don't know how long that will last. I was just wondering if anybody knew someplace I could look to maybe find a buyer. Thanks
Reply With Quote
  #2 (permalink)  
Old 11-22-2007, 10:12 PM
sdold's Avatar
Amateur Metal Finisher
 
Join Date: Jul 2005
Posts: 221
sdold is on a distinguished road
Default Re: Hey guys.....

Advertise it on Craigslist. I've found Craigslist to be a lot easier to sell big things on than ebay. It's the only place I look for big stuff anymore.
__________________
Steve Dold
http://stevedold.com
Reply With Quote
  #3 (permalink)  
Old 11-24-2007, 06:44 PM
Amateur Metal Finisher
 
Join Date: Jul 2006
Posts: 222
ed_denu is on a distinguished road
Default Re: Hey guys.....

Post a notice on the Eastwood powder coat forum.
Reply With Quote
  #4 (permalink)  
Old 11-28-2007, 03:31 PM
nuttyman's Avatar
Metal Finishing Guru
 
Join Date: Sep 2003
Location: Rio Rancho, NM
Posts: 553
nuttyman
Default Re: Hey guys.....

hey old dude--how big is it? what are the dimensions?
__________________
SouthWest Powderworx
Tyler Nutter
5054803934
www.swpowder.com
myspace/swpowder
tyler@swpowder.com
Reply With Quote
  #5 (permalink)  
Old 11-30-2007, 08:34 AM
Newbie
 
Join Date: Aug 2006
Posts: 20
olddude is on a distinguished road
Default Re: Hey guys.....

It's pretty big roughly 8x8x8. It has 4" mineral wool in all walls including floor and when I fired it up fora test run it came up to temp 400 degrees in about 20 minutes. I never did get a chance to completely finish it because we moved. I Srink wraped it and stored it for a year outside but now it is in inside storage but I still cannot hook it up because of power limitations.

It has one big door that needs to be re-installed the hinges need to be remounted. When I installed them I was by myself and the door almost fell on me so I welded them where I could get them. They just need to be flipped around and wouldn't take long to grind them off and re-install them one at a time the right way. The air pipe is on the outside and needs to be insulated and attached from the fan to the air box.

It has three big electric burners mounted in the floor. I'll have to check the wattage because I can't remember how big they are but they are enough to do the job. Maybe I'll take some pics and post them but mainly I was wondering what to ask for something like this.
Reply With Quote
  #6 (permalink)  
Old 12-01-2007, 02:29 PM
Newbie
 
Join Date: Aug 2006
Posts: 20
olddude is on a distinguished road
Default Re: Hey guys.....

Quote:
Originally Posted by nuttyman View Post
hey old dude--how big is it? what are the dimensions?
I posted some pics in the members gallery, I couldn't figure out how to get them here. I posted that it was 8x8x8 but in reality it is 8 high X 7'4" wide X
7'4" deep on the inside.
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
For all you paintball guys... hvacman250 Anodizing Questions 6 08-07-2007 12:29 PM
guys tell me what u think Empire03 Anodizing Questions 5 07-19-2007 02:08 PM
For the paintball guys... hvacman250 Anodizing Questions 8 05-17-2007 12:44 AM
Thanks Guys, but im out..... johnny933 Powder Coating Questions 1 02-28-2005 10:25 PM
What gun are you guys using for PC? Fudd Powder Coating Questions 3 12-07-2003 12:08 PM


All times are GMT -4. The time now is 12:15 AM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.