maybe! you'll have to test it out. you might be just on the edge of not enough volume. If you are going to use an air hose to feed it use a hose no longer than 25' of a 1/2" hose. I have a 10HP 120 gallon tank & I have no issues.
__________________
SouthWest Powderworx Tyler Nutter 5054803934 www.swpowder.com myspace/swpowder tyler@swpowder.com |
|
||||
|
I'll set the cab within 10 feet of the compressor and give it a whirl. Reclaim/dust box is back ordered 20 days they says, darn!
__________________
GatorHyde of Denver 10650 Irma Dr. #24 Northglenn, CO 80233 303 280-3056 |
|
||||
|
that's what they told me. 3 1/2 months later it arrived.
__________________
SouthWest Powderworx Tyler Nutter 5054803934 www.swpowder.com myspace/swpowder tyler@swpowder.com |
|
||||
|
I hope that doesn't happen to me, or I will HAVE to wreck my shop vac. If the compressor isn't gonna work, I get a big one, try what I have first. Do you have the part numbers for ordering this 3 month wait "tips"?
Alex
__________________
GatorHyde of Denver 10650 Irma Dr. #24 Northglenn, CO 80233 303 280-3056 |
|
||||
|
not anymore. I called customer service/parts & referenced the blast cabinet part #.
__________________
SouthWest Powderworx Tyler Nutter 5054803934 www.swpowder.com myspace/swpowder tyler@swpowder.com |
|
||||
|
you can get a shop vac cyclone on ebay for under $100 shipped. it goes in-line between the shop vac and cabinet and works amazing. nothing gets through to the vac and there's nothing to ever get clogged. if you just use it for the cabinet, i'm sure you can reclaim a good bit of the media. search "cyclone separator" in ebay.
__________________
Len Figure Engineering, LLC |
![]() |
| Bookmarks |
| Currently Active Users Viewing This Thread: 1 (0 members and 1 guests) | |
| Thread Tools | |
| Display Modes | |
|
|
Similar Threads
|
||||
| Thread | Thread Starter | Forum | Replies | Last Post |
| dust collector on blast cabinet? | shamrox | Powder Coating Questions | 13 | 06-05-2008 11:21 PM |
| road to a new blast cabinet | krymis | Other Metal Finishing Questions | 6 | 09-11-2007 01:15 AM |
| How's the TP tool's 770 (skat) blast cabinet | sal1355 | Other Metal Finishing Questions | 0 | 12-31-2006 03:28 PM |
| Incandesent lighing in blast cabinet | ottoplex | Powder Coating Questions | 1 | 09-10-2006 10:05 PM |
| building a blast cabinet from scratch | 11111111 | Powder Coating Questions | 10 | 05-11-2004 04:59 PM |