Caswell Inc. Metal Finishing Forums  

Go Back   Caswell Inc. Metal Finishing Forums > Powder Coating Questions > Oven Building Forum
Connect with Facebook


Oven Building Forum Building A Curing Oven? - Here's the place to post your questions, specs and ideas.

Reply
 
LinkBack Thread Tools Display Modes
  #1 (permalink)  
Old 07-04-2008, 10:30 PM
Newbie
Caswell Platinum Member
 
Join Date: Apr 2008
Posts: 14
peak-j is on a distinguished road
Default Just finished building an oven

Here are a few pics of the oven I built, just coated a few scraps setting around. Trying to figure it all out now.


Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
Reply With Quote
  #2 (permalink)  
Old 07-04-2008, 10:33 PM
Newbie
Caswell Platinum Member
 
Join Date: Apr 2008
Posts: 14
peak-j is on a distinguished road
Default Re: Just finished building an oven

Couple pieces I did today, wasn't to bad for the first time doing it I guess.

Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
Reply With Quote
  #3 (permalink)  
Old 07-06-2008, 09:38 PM
JTW37's Avatar
Metal Finishing Guru
Caswell Platinum Member
 
Join Date: Feb 2006
Location: Bristol, In
Posts: 691
JTW37 is an unknown quantity at this point
Default Re: Just finished building an oven

Oven looks okay, work looks okay as well. Can't see it real good, but for the first time, I would say at least an A for effort.
__________________
Who says you can't teach an ole dog new tricks?
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
Reply With Quote
  #4 (permalink)  
Old 07-12-2008, 09:55 AM
Experienced Metal Finisher
 
Join Date: May 2008
Posts: 252
Grumple is on a distinguished road
Default Re: Just finished building an oven

Looks good. What size is it? What controller and elements are you using?
__________________
Grumple
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
Reply With Quote
  #5 (permalink)  
Old 07-12-2008, 06:37 PM
Newbie
Caswell Platinum Member
 
Join Date: Apr 2008
Posts: 14
peak-j is on a distinguished road
Default Re: Just finished building an oven

It is 40"x40"x60", the rest of it is out of an old cook stove. Nothing special but so far it is working.
Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off


Similar Threads
Thread Thread Starter Forum Replies Last Post
Finally finished my PC curing oven!!! ...and one question x1rider Powder Coating Questions 12 07-08-2008 05:22 AM
Finished my oven--some pics too nuttyman Oven Building Forum 41 05-17-2008 05:00 PM
Finished Oven!!! Well Almost kg4mon Oven Building Forum 5 04-10-2008 03:40 PM
7/8 finished oven for sale tiller11875 Oven Building Forum 3 05-29-2007 12:34 PM
Oven Building hd-ryder Oven Building Forum 0 04-16-2004 10:52 AM


All times are GMT -4. The time now is 08:20 AM.