Default Hobby oven pic

Finished wiring this AM, heats to 380deg in 8 minutes and holds at 380deg. Used PID, T/C and SSR from Auber ins, very helpfull via e-mail. I also installed a heat sink and cooling fan, the fan is on the right side and blows directly on the SSR. Thank you for all the help recieved on this forum.
Terry
Attached Thumbnails
hobby-oven-pic-oven-001.jpg  
Reply With Quote
  #2 (permalink)  
Old 07-25-2008, 12:13 PM
Amateur Metal Finisher
 
Join Date: Jul 2007
Location: Western WA.
Posts: 60
PhredAre is on a distinguished road
Default Re: Hobby oven pic

Looks good ! Well thought out. Hopefully the PID won,t get too hot in its location directly above the Oven. Fred

Last edited by PhredAre; 07-25-2008 at 12:18 PM.
Reply With Quote
  #3 (permalink)  
Old 07-25-2008, 11:57 PM
Newbie
 
Join Date: Jul 2008
Posts: 25
cessna182 is on a distinguished road
Default Re: Hobby oven pic

Thanks for the comments PhredAir, good point on the pid temp, today I put temp pickup at the pid, will check temp next bake.
Terry
Reply With Quote
  #4 (permalink)  
Old 07-29-2008, 05:24 AM
JTW37's Avatar
Metal Finishing Guru
Caswell Platinum Member
 
Join Date: Feb 2006
Location: Bristol, In
Posts: 517
JTW37 is an unknown quantity at this point
Default Re: Hobby oven pic

Always good to see someone finish their oven successfully. Looks good. Hope it works out for you.
__________________
Who says you can't teach an ole dog new tricks?
Reply With Quote
Reply

Bookmarks


Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
 
Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Trackbacks are Off
Pingbacks are Off
Refbacks are Off

Similar Threads
Thread Thread Starter Forum Replies Last Post
Your 50KV Hobby Gun needs....... NXGHOST Caswell Please Sell This... 2 05-25-2007 01:06 AM
Hobby gun gasket harleyman Powder Coating Questions 1 12-15-2006 08:37 AM
Better fluidizing in the hobby gun? cruizer Powder Coating Questions 15 09-21-2006 06:13 PM
Hobby vs Pro customandsound Powder Coating Questions 6 07-08-2005 01:56 PM
From hobby to Job getastro Powder Coating Questions 12 02-06-2005 08:54 AM


All times are GMT -4. The time now is 11:20 PM.


Powered by vBulletin® Version 3.7.3
Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Search Engine Friendly URLs by vBSEO 3.2.0 RC4
Copyright © Caswell Inc.