+ Reply to Thread
Page 4 of 6
FirstFirst ... 2 3 4 5 6 LastLast
Results 31 to 40 of 55

Thread: My propane fired oven build

  1. #31

    Default Re: My propane fired oven build

    Hi there I want to cure powder coating and ceramic that's the reason I ask If the oven makes temperatures over 650f with the 55,000 btu's propane heater.
    the other question if the air come out of the heater if strong or not. Thank you very much Big Toy for your Time.
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  2. #32
    Join Date
    May 2009
    Location
    Veneta,OR
    Posts
    24

    Default Re: My propane fired oven build

    Quote Originally Posted by Cronox View Post
    Hi there I want to cure powder coating and ceramic that's the reason I ask If the oven makes temperatures over 650f with the 55,000 btu's propane heater.
    the other question if the air come out of the heater if strong or not. Thank you very much Big Toy for your Time.
    I see. I think most ceramics cure around 500f. Maybe this weekend I will see how hot I can get the oven. There really is not that much air that comes out the exhaust. Not all of the air from the blower on the heater enters the oven.
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  3. #33
    Join Date
    May 2009
    Location
    Veneta,OR
    Posts
    24

    Default Re: My propane fired oven build

    So I finally got around to testing the upper temps for the oven. After I got done with a few parts I cranked the pid up to 600F.

    400-500...10min
    500-500...10min
    550-600...10min

    So, it went from 75 to 600F in about 45 minutes. out side oven temp on the wall was about 95F.
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  4. #34
    Join Date
    Sep 2005
    Location
    South Texas
    Posts
    886

    Default Re: My propane fired oven build

    Hot diggity! That's a toasty oven!

    How well does it HOLD the temps?
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  5. #35
    Join Date
    May 2009
    Location
    Veneta,OR
    Posts
    24

    Default Re: My propane fired oven build

    Quote Originally Posted by CarWiz View Post
    Hot diggity! That's a toasty oven!

    How well does it HOLD the temps?
    It has to work pretty hard to keep 600F. Maybe 80% duty cycle. At 400F it only about 25% duty cycle.
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  6. #36

    Default Re: My propane fired oven build

    Bigtoy:
    Nice job on the oven!!
    I have one of those PID's on my electric oven (5'x5'x7'), works great as far as accuracy, probably overkill but I can also use the same oven with other programed temp curves to mold plexiglass.
    Question..I am building a big propane oven (8'x8'x24'), the pid on the electric oven turns the power on and off very rapidly when near or at set point, like on 1 sec. off 1 sec. on 1 sec...... , SSR's can handle that. Does yours turn the gas on and off often? If so have you worried about lifespan of the valve?
    Morgan
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  7. #37
    Join Date
    Jul 2006
    Posts
    738

    Default Re: My propane fired oven build

    PID's normally have a 'cycle rate' parameter that allows you to control the frequency of the on/off cycling. My pid goes to 199 seconds.

    Only issue would be maintaining the set temperature if the cycle rate were set to high.
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  8. #38

    Default Re: My propane fired oven build

    Thanks Ed, I will look for the cycle rate setting, I guess I missed it last time.
    Morgan
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  9. #39
    Join Date
    May 2009
    Location
    Veneta,OR
    Posts
    24

    Default Re: My propane fired oven build

    It does cycle pretty fast. On for a few seconds off for a few seconds. When the oven heat soaks for a wile it does no cycle as much. I am not too worried about wearing out the valve. It is cheap.
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

  10. #40

    Default Re: My propane fired oven build

    Do you have a brand and part number or more specs on the valve? You say its cheap but when I google "gas valve" I get stuff $40-$400 on up. Any other words of wisdom for someone trying to wire one up? Thanks.
    Digg this Post!Add Post to del.icio.usBookmark Post in TechnoratiFurl this Post!
    Reply With Quote Reply With Quote  
    Share with Facebook

+ Reply to Thread
Page 4 of 6
FirstFirst ... 2 3 4 5 6 LastLast

Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

     

Similar Threads

  1. Anyone built a natural gas fired oven?????
    By asalony in forum Oven Building Forum
    Replies: 0
    Last Post: 05-21-2008, 05:38 PM
  2. oven build/ elec IR/ or propane IR?
    By Carcher7878 in forum Oven Building Forum
    Replies: 8
    Last Post: 04-06-2007, 04:29 PM
  3. Gas fired oven in central PA or Northern MD
    By datadawg in forum Oven Building Forum
    Replies: 2
    Last Post: 05-10-2006, 08:39 PM
  4. Gas fired oven
    By dfarning in forum Oven Building Forum
    Replies: 5
    Last Post: 04-12-2006, 09:40 PM
  5. Gas fired pizza oven for curing?
    By BlindUmpire in forum Oven Building Forum
    Replies: 4
    Last Post: 02-27-2004, 11:21 PM

Bookmarks

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts

Search Engine Friendly URLs by vBSEO 3.5.0 RC1 PL1