Caswell Inc. Metal Finishing Forums  

Connect with Facebook

Notices

  Home · Search · Register  

Statistics
Users 78,975
Photos 2,912
Comments 939
Views 25,895,249
Disk Space 510.5mb

« November 2009
SunMon TueWed ThuFri Sat
1234567
891011121314
15161718192021
22232425262728
2930     

Random Images - Nickel & Gold Plating Photos
V_004.jpg
Gold Plated Guitar P
jg

[ Nickel & Gold Plating Photos ]
V_003.jpg
Gold Plated Guitar P
jg

[ Nickel & Gold Plating Photos ]
V_002.jpg
Gold Plated Guitar P
jg

[ Nickel & Gold Plating Photos ]
V_001.jpg
Gold Plated Guitar P
jg

[ Nickel & Gold Plating Photos ]
· more ·

 
Home » Member » jg » Nickel & Gold Plating Photos Photo Options
V_001.jpg
V_002.jpg
V_003.jpg
V_004.jpg

Previous image   Slide Show   Next image

Gold Plated Guitar Parts
Click on image to view larger image

Previous image   Slide Show   Next image


Photo Details
jg



Newbie

Registered: February 2003
Posts: 4
users gallery
Pickup bezels and selector switch knob machined from brass and nickel/gold tank plated. Tremolo base gold plating redone with nickel/gold tank plating. Tremolo string lock screws and fine tuning screws nickel/gold tank plated. String saddle, jack plate, and tremolo arm gold plating redone.
· Date: Fri April 3, 2009 · Views: 1480
· Filesize: 30.6kb, 172.5kb · Dimensions: 1000 x 606 ·
Additional Info
Quick Rate: Poor Excellent
Keywords: nickel gold plated guitar parts



Photo Sharing Gallery by PhotoPost
Copyright © 2007 All Enthusiast, Inc.


All times are GMT -4. The time now is 05:21 PM.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2009, Jelsoft Enterprises Ltd.
Copyright © Caswell Inc.