Here a couple of pics of my first time results with the Caswell kit. Nothing short of spectacular. Just followed the directions to the letter and viola, perfect results. Plated to raw steel and no polishing was required. Plated to .001" due to exposer to road conditons. Could not be more pleased. Thanks to Caswell.